EVA agricultural film
EVA agricultural film

Features:
1. Blow molding, on-line coating, width 4-16 meters;
2. Add metallocene linearity, taking into account film strength and heat preservation;
3. The effect of dripping and anti-fog is synchronized with the service life of the film;
4. High effective light transmittance and excellent dustproof effect.
5. For continuous fog sheds and greenhouse sheds with high requirements for anti-fog, dripping light transmission and heat preservation effect, it can be used continuously for many years.

EVA agricultural film materials and processing technology:
The research and development and launch of EVA agricultural film draws on the accumulation of EVA coated thin film technology in foreign countries for nearly 10 years, making full use of the characteristics of EVA resin, and using the matching ratio reasonably, that is, taking into account the good toughness of EVA resin and low temperature resistance. The thermal properties of the material and the material itself improve the strength of the film.
EVA agricultural film is blown and produced by three-layer co-extrusion technology. The width can reach 18 meters (depending on the thickness). The coating equipment is introduced and the coating effect is uniform. The self-developed light-heat drying system ensures the film coating effect and Film flatness.

Precautions for EVA agricultural film laying:
1) EVA agricultural film coating should pay special attention to protect the coating layer from dragging and rubbing to damage the coating layer, causing local droplet failure function;
2) The coating layer is a high-tech hydrophilic material, pay attention to prevent oil pollution, and affect the effect of droplets and fog elimination;
3) In the initial stage of coating the film, the moisture in the shed may not be sufficient, and the inner surface of the film may not form a complete water film layer, and the tiny water droplets hinder the light during a short period of time. However, as the temperature and humidity in the shed increase, the phenomenon disappears completely after the formation of the water film.